Because East German industry urgently needed coke after the Second World War and the anthracite coal traditionally used for its production was found for the most part in western Germany, the two process engineers Erich Rammler and Georg Bilkenroth began researching and developing a metallurgical high-temperature lignite coke in 1949. This could be used for iron production, non-ferrous metallurgy and carbide production.
The two scientists of the Bergakademie Freiberg concentrated their research on the Lower Lusatian lignite and in 1952 were finally able to obtain a patent for Lignite high-temperature gasification.
The coke was produced both as bulk material and in briquette form.
Production facilities
From 1952, the high temperature lignite coke was produced in the large coking plant VEB Braunkohleveredelung Lauchhammer and later also in the coking plant at VEB Gaskombinat Schwarze Pumpe. By-products of lignite coking are tar, medium oil and light oil as well as high-quality natural gas.